        <title>Etching Acetal (Delrin) plastic in preparation for painting, gluing, etc</title>
        <link>https://tube.loping.net/videos/watch/953ca69f-1436-42a4-988c-2498830918d5</link>
        <description>I mixed: 40g water 25g potassium dichromate 500g concentrated sulfuric acid http://books.google.com/books?id=Fl57Byhp0ecC&amp;lpg=PA114&amp;ots=wYk-A7i9px&amp;dq=delrin%20etch%20chemical&amp;pg=PA114#v=onepage&amp;q=delrin%20etch%20chemical&amp;f=false I guess this mixture is commonly called chromic acid. Things that I should have done: Use a Pyrex beaker Don't use the magnetic stirrer, just use a teflon stir stick Use an ice bath at the beginning of the procedure</description>
        <lastBuildDate>Sun, 12 Jul 2026 14:23:36 GMT</lastBuildDate>
        <docs>https://validator.w3.org/feed/docs/rss2.html</docs>
        <generator>PeerTube - https://tube.loping.net</generator>
        <image>
            <title>Etching Acetal (Delrin) plastic in preparation for painting, gluing, etc</title>
            <url>https://tube.loping.net/lazy-static/avatars/8a56e488-2120-4649-a417-badf5893657b.png</url>
            <link>https://tube.loping.net/videos/watch/953ca69f-1436-42a4-988c-2498830918d5</link>
        </image>
        <copyright>All rights reserved, unless otherwise specified in the terms specified at https://tube.loping.net/about and potential licenses granted by each content's rightholder.</copyright>
        <atom:link href="https://tube.loping.net/feeds/video-comments.xml?videoId=953ca69f-1436-42a4-988c-2498830918d5" rel="self" type="application/rss+xml"/>
    </channel>
</rss>